metricas
covid
Boletín de la Sociedad Española de Cerámica y Vidrio Processing, nanoindentation and scratch testing of alumina-coated YTZP
Journal Information

Statistics

Follow this link to access the full text of the article

Processing, nanoindentation and scratch testing of alumina-coated YTZP
Procesamiento, nanoindentación y rayado de materiales de YTZP recubiertos con alúmina
Jorge Vallea,b, Marc Angladab, Begoña Ferraria, Carmen Baudína,
Corresponding author
cbaudin@icv.csic.es

Corresponding author.
a Instituto de Cerámica y Vidrio, CSIC, Madrid, Spain
b Department of Materials Science and Engineering/ETSEIB, Barcelona, Spain
Read
5813
Times
was read the article
1343
Total PDF
4470
Total HTML
Share statistics
Article information
ISSN: 03663175
Original language: English
The statistics are updated each day
Year/Month Html Pdf Total
2025 12 92 36 128
2025 11 52 36 88
2025 10 37 27 64
2025 9 36 21 57
2025 8 33 11 44
2025 7 44 6 50
2025 6 25 10 35
2025 5 35 4 39
2025 4 33 4 37
2025 3 31 4 35
2025 2 32 0 32
2025 1 27 1 28
2024 12 32 3 35
2024 11 19 1 20
2024 10 18 4 22
2024 9 27 2 29
2024 8 22 3 25
2024 7 18 2 20
2024 6 16 2 18
2024 5 20 1 21
2024 4 18 10 28
2024 3 25 9 34
2024 2 11 1 12
2024 1 35 7 42
2023 12 36 9 45
2023 11 43 10 53
2023 10 61 11 72
2023 9 23 5 28
2023 8 25 12 37
2023 7 20 10 30
2023 6 23 12 35
2023 5 43 7 50
2023 4 53 3 56
2023 3 52 1 53
2023 2 52 6 58
2023 1 50 4 54
2022 12 48 9 57
2022 11 51 22 73
2022 10 49 8 57
2022 9 41 7 48
2022 8 33 11 44
2022 7 33 10 43
2022 6 32 11 43
2022 5 32 6 38
2022 4 29 9 38
2022 3 42 22 64
2022 2 49 13 62
2022 1 66 7 73
2021 12 42 19 61
2021 11 27 8 35
2021 10 39 15 54
2021 9 34 17 51
2021 8 43 7 50
2021 7 36 15 51
2021 6 36 12 48
2021 5 48 7 55
2021 4 117 32 149
2021 3 44 14 58
2021 2 48 10 58
2021 1 54 21 75
2020 12 51 18 69
2020 11 37 18 55
2020 10 29 12 41
2020 9 19 18 37
2020 8 35 4 39
2020 7 19 13 32
2020 6 26 10 36
2020 5 22 4 26
2020 4 20 11 31
2020 3 22 4 26
2020 2 24 5 29
2020 1 24 7 31
2019 12 26 7 33
2019 11 26 8 34
2019 10 30 7 37
2019 9 21 12 33
2019 8 19 3 22
2019 7 22 9 31
2019 6 61 28 89
2019 5 121 26 147
2019 4 63 28 91
2019 3 13 13 26
2019 2 24 9 33
2019 1 13 9 22
2018 12 22 8 30
2018 11 49 21 70
2018 10 36 17 53
2018 9 17 22 39
2018 8 13 1 14
2018 7 7 6 13
2018 6 19 6 25
2018 5 20 2 22
2018 4 9 0 9
2018 3 8 0 8
2018 2 18 11 29
2018 1 20 2 22
2017 12 13 0 13
2017 11 20 0 20
2017 10 19 6 25
2017 9 18 0 18
2017 8 9 5 14
2017 7 13 6 19
2017 6 26 6 32
2017 5 23 1 24
2017 4 18 0 18
2017 3 19 25 44
2017 2 20 12 32
2017 1 16 3 19
2016 12 50 8 58
2016 11 61 10 71
2016 10 59 7 66
2016 9 66 8 74
2016 8 62 5 67
2016 7 54 2 56
2016 6 52 14 66
2016 5 36 23 59
2016 4 44 17 61
2016 3 64 25 89
2016 2 50 25 75
2016 1 78 21 99
2015 12 45 23 68
2015 11 59 27 86
2015 10 84 40 124
2015 9 77 26 103
2015 8 18 12 30
Show all

Follow this link to access the full text of the article

Article options
Tools